EMPREGO DE TELAS DE AÇO INOXIDÁVEL 304 E TITÂNIO COMO CATODOS PARA RECUPERAÇÃO DE METAIS DE EFLUENTES DE CIANÍDRICOS DE MINERAÇÃO DE OURO

USE OF 304 STAINLESS STEEL AND TITANIUM MESHES AS CATHODES FOR RECOVERY OF METALS FROM GOLD MINING CYANIDE EFFLUENTS

DOI

10.5151/2594-5327-16234

Downloads

Baixar Artigo 11 Downloads

Resumo

O presente trabalho apresenta um estudo comparativo entre telas de aço inoxidável e de titânio, como catodo, com vistas no desempenho energético e nas taxas de remoção de metais. Foram empregadas ferramentas estatísticas visando à identificação das variáveis significativas no processo de recuperação eletrolítica de ouro, prata e cobre e oxidação do cianeto de efluentes da mineração de ouro. Para uma solução sintética contendo respectivamente 0,5 mg/L de ouro, 7,5 mg/L de prata, 150mg/L de cobre e 150 mg/L de cianeto livre, empregando-se catodos de aço inoxidável após 180 minutos de eletrólise, foram obtidas remoções de cobre e prata em torno de 99,6% e 95,5%, respectivamente, além da completa remoção do ouro. Com catodos de titânio, nas mesmas condições, a recuperação de cobre foi de 99,3%, além da completa remoção do ouro e da prata. Em ambos os casos, a oxidação de cianeto ficou próxima a 99%. O consumo energético específico médio obtido com o catodo de titânio foi de 66,19 kWh/kg de metal, enquanto que com o de aço inoxidável foi de 88,29 kWh/kg.

 

With titanium cathodes under the same conditions, the copper recovery was 99.3%, and the complete removal of gold and silver were obtained. In both cases, the oxidation of cyanide was close to 99%. The average specific energy consumption obtained for the titanium cathode was 66.19 kWh/kg of metal, while for stainless steel as 88.29 kWh/kg. This paper presents a comparative study between stainless steel and titanium meshes to be used as cathodes, aiming at high metal recovery rates and good energetic performance. Statistical tools were used in order to identify the significant variables in the electrolytic recovery of gold, silver and copper and cyanide oxidation from gold mining wastewaters. For a synthetic solution containing respectively 0.5 mg/L gold, 7.5 mg/L silver, 150 mg/L copper and 150 mg/L free cyanide, after 180 minutes of electrolysis, using stainless steel cathodes copper and silver removals of 99.6% and 95.5%, respectively, were obtained besides the complete removal of gold.

Palavras-chave

Cianeto; Cobre; Efluentes; Processo eletrolítico.

Cyanide; Copper; Effluents; Electrochemical process.