ESTUDO DO PADRÃO DE ROMPIMENTO E DA FORÇA DE DESLIGAMENTO DOS FILAMENTOS DO BISSO DO Limnoperna fortunei (DUNKER, 1857) EM DIFERENTES TIPOS DE SUBSTRATOS

STUDY OF THE PATTERN OF DISRUPTION AND DETACHMENT FORCE OF THE BYSSUS FILAMENTS Limnoperna fortunei (Dunker, 1857) IN DIFFERENT TYPES OF SUBSTRATES

DOI

10.5151/2594-5327-21565

Downloads

Baixar Artigo 128 Downloads

Resumo

O Limnoperna fortunei é um molusco bivalve invasor que tem causado prejuízos a sistemas de captação de água e usinas hidroelétricas. Sua presença já foi registrada nas bacias dos rios Paraná, Paraguai, Uruguai e Lago Guaíba. Neste trabalho, estudou-se a força de desligamento e o padrão de rompimento dos filamentos do bisso do L.fortunei em três tipos de substratos: cobre, vidro e teflon. O cobre provocou efeito letal em 100% dos mexilhões. A maior parte dos filamentos do bisso analisados se desprendeu dos substratos (vidro e teflon) por rompimento. A falha adesiva ocorreu em 20% dos filamentos que estavam aderidos ao teflon. Os filamentos do bisso aderidos ao vidro e ao teflon romperam em duas regiões distintas: X e Y. Quanto aos tipos de rompimento foram observados dois padrões distintos: superfície estirada de ruptura tipo estricção e superfície plana de ruptura transversal. A região de rompimento dos filamentos do bisso pode estar relacionada com as características estruturais das regiões X e Y não com o tipo de substrato. O substrato parece influenciar os tipos de rompimento e a força de desligamento. Esta apresentou maior valor para os mexilhões aderidos ao vidro em relação ao teflon.

 

The Limnoperna fortunei is a freshwater bivalve invader that has caused damage to water catchment systems and hydroelectric plants. His presence has already been recorded in the basins of the rivers Parana, Paraguay, Uruguay and Guaíba Lake. In this present work, was conducted a study about the detachment force and pattern of disruption of the byssus filaments on different substrates. Three types of materials were selected (copper, teflon and glass). Copper had a lethal effect on a 100% of the tested mussels. The adhesive failure occurred only in the Teflon. The byssus filaments adhered to glass and teflon disrupted in two distinct regions: X (next to the body) and Y (away/far from the body). Also there were observed, on these filaments, two distinct types of disruption: stretched surface rupture and flat surface transverse rupture. The region of disruption of the filaments of byssus seems related to the structural characteristics of regions X (next to the body) e Y (away/far from the body) and not with the type of substrate. The substrate appears to influence the kinds of disruption and detachment force. This presents a greater value for the mussels attached to glass compared to Teflon.

Palavras-chave

Bisso; Mexilhão dourado; Padrão de rompimento; Força de desligamento.

Byssus; Disrupture pattern; Golden mussel; Detachment force.

Como citar

Duarte, Madrith Sthel Costa; Froes, Claudia Lauria; Custódio, Gislene; Branco, José Roberto Tavares. ESTUDO DO PADRÃO DE ROMPIMENTO E DA FORÇA DE DESLIGAMENTO DOS FILAMENTOS DO BISSO DO Limnoperna fortunei (DUNKER, 1857) EM DIFERENTES TIPOS DE SUBSTRATOS , p. 3829-3841. In: 67º Congresso da ABM - Internacional / 12º ENEMET - Encontro Nacional de Estudantes de Engenharia Metalúrgica, de Materiais e de Minas, Rio de Jabeiro, 2012.
ISSN: 2594-5327 , DOI 10.5151/2594-5327-21565