Resumo

No mix de produtos laminados a frio da COSIPA, encontram-se materiais com alta performance de limpeza, denominados ''Extra-Limpo''. Estes produtos possuem características de alta refletância, com baixos níveis de carbono residual e ferro sobre a chapa. Como conseqüência da tendência mundial por melhoria da qualidade, ocorreu um forte aumento na demanda por produtos com exigências de maior limpeza superficial, requisitados por uma ampla gama de clientes, das mais variadas aplicações. Inicialmente produzidas com espessuras entre 0,60mm a 0,80mm e larguras até 1250mm, passou-se a demandar espessuras mais finas, chegando a 0,38mm e larguras desde 800 mm a 1580 mm. Visando atender a estas exigências do mercado, foi necessário efetuar desenvolvimentos e ajustes nos parâmetros de processo para atender esta qualidade em dimensões criticas. Foi utilizado o método matricial objetivando melhorar a performance do processo, reduzir o índice de desvios e aumentar a capabilidade de produção no Laminador de Tiras a Frio e Recozimento, de modo a garantir a limpeza superficial requerida pela especificação Extra-Limpo para essas dimensões.

 

Within Cosipa cold rolled product mix it has been processed materials with high cleanliness performance called extra-clean materials. These products exhibit high reflectance features, achieving low level of residual carbon and iron on the strip surface. Following a global trending towards quality, it was observed a strong marked demand for products with high surface cleanliness, required by a large range of costumers, from the most varied application. Firstly manufactured with thickness between 0.60 mm and 0.80 mm and width until 1250 mm, they are now demanded thickness as thinner as 0.38 mm and width ranging from 800 mm to 1580 mm. Aiming to supply these materials to the new pressing customer, it was necessary to make new developments and to adjust procedures in order to assure the best quality to the critical dimensions. It was implemented a matrix method aiming to improve the process performance, to increase the yield level and process capability of the tandem cold mill and annealing lines, in order to guarantee the high strip cleanliness required by the extra-clean specification to this broad product spectrum.

Palavras-chave

Refletância; Sistemas de refrigeração; Limpeza superficial.

Reflectance; Roll coolant systems; Surface cleanliness.

Como citar

Melo, Francisco Gomes de; Dantas, José Valdir Amorim; Bagger, Karl Kristian; Silva, Lucio Rosa da; Pereira, Marcelo Magalhães. DESENVOLVIMENTO DO PROCESSO DE PRODUTO EXTRA-LIMPO COM DIMENSÕES CRÍTICAS , p. 511-519. In: 43º Seminário de Laminação, Processos e Produtos Laminados e Revestidos, São Paulo, 2006.