Powered by Blucher Proceedings

Proceedings of ABM Annual Congress


ISSN 2594-5327

70th ABM Annual Congress — Vol. 70 , num. 70 (2015)


Title

ANÁLISE DE FALHA DE GARFOS DE EMPILHADEIRA FRATURADOS DURANTE LEVANTAMENTO DE CARGA

FAILURE ANALYSIS OF FORKLIFT FORKS FRACTURED DURING LOAD LIFTING

Authorship

DOI

10.5151/1516-392X-26485

Downloads

2490 Downloads

Abstract

Empilhadeiras são equipamentos essenciais na movimentação de cargas em praticamente qualquer ambiente industrial e devem receber atenção especial em caso de falhas, pois podem comprometer operações e colocar em risco a saúde e a segurança de colaboradores. Este trabalho apresenta uma análise de falha dos garfos de uma empilhadeira que romperam durante uma operação rotineira de levantamento de carga. Amostras dos garfos fraturados foram submetidas à análise química, análise macrográfica, micrografia óptica, análises de dureza e microdureza e ensaios de tração e impacto. Além disso, foram analisadas as tensões as quais os garfos estavam submetidos, considerando a carga levantada, a especificação do equipamento e análises de fadiga e de tenacidade à fratura. Dessa maneira foi possível identificar o material dos garfos, suas características e também de que maneira ocorreu a fratura, resultando em recomendações que possam prever e/ou evitar ocorrências desse tipo futuramente.

 

Forklifts are essential equipment in cargo handling in virtually any industrial environment and should receive special attention in case of failure, because they may compromise operations and the health and safety of employees. This paper presents a failure analysis of the forks of a forklift that broke during a routine operation of load lifting. Samples of the fractured forks were subjected to chemical analysis, macrographic analysis, optical micrography, hardness and microhardness analysis and tensile and impact tests. Additionally, the tensions which the forks were subjected to were analyzed, considering the load being lifted, the specification of the equipment and analysis of fatigue and fracture toughness. This way it was possible to identify the material of the forks, its characteristics and also how the fracture occurred, resulting in recommendations that may predict and / or prevent such occurrences in the future.

Keywords

Análise de falha, Fadiga, Tenacidade à fratura, Inspeção

Failure analysis, Fatigue, Fracture toughness, Inspection

How to cite

Grilo, André de Almeida; Milan, Marcelo Tadeu; Guastala, Fábio Arielo. ANÁLISE DE FALHA DE GARFOS DE EMPILHADEIRA FRATURADOS DURANTE LEVANTAMENTO DE CARGA, p. 982-991. In: 70th ABM Annual Congress, Rio de Janeiro, 2015.
ISSN: 2594-5327, DOI 10.5151/1516-392X-26485