At thyssenkruppCSA, a positive heat balance at BOF process is faced, mainly because of low utilization of scrap and plant design. A singular logistic concept for hot metal transport between blast furnace and steel plant was established to optimize transportation and energy balance. Up to 80 kg of iron ore pellets/t steel is necessary for 340t BOF heat balance. In order to accomplish this challenge a stable blowing process, intensive operational development have been successfully executed: slopping rate reduction of 80% achieved without changing the blowing time. This paper describes steps and results of this development.
Keywords
BOF, LD converter, process, slopping, iron ore, addition, blowing process
BOF, LD converter, process, slopping, iron ore, addition, blowing process
How to refer
Carvalho, Daniel Augusto Godinho de;
Castro, Herbert;
Demuner, Leonardo;
Viana, Marcos;
Wojnar, Pavel;
Schulz, Tilo;
Maia, Breno Totti.
BOF BLOWING PROCESS CHALLENGES FOR HIGH RATE OF IRON ORE PELLET ADDITION - PROCESS DEVELOPMENT AND RESULTS AT TKCSA
,
p. 637-645.
In: 48º Seminário de Aciaria, Fundição e Metalurgia de Não-Ferrosos,
São Paulo,
2017.
ISSN: 2594-5300
, DOI 10.5151/1982-9345-30634