Proceedings of the Ironmaking, Iron Ore and Agglomeration Seminars


ISSN 2594-357X

37º Redução e 8º Minério de Ferro vol. 2, num.2 (2007)


Title

DEPRESSÃO DE MINERAIS DE FERRO: INFLUÊNCIA DA MINERALOGIA, MORFOLOGIA E pH DE CONDICIONAMENTO

IRON ORE MINERALS DEPRESSION: INFLUENCE OF MINERALOGY, MORPHOLOGY AND pH CONDITIONING

DOI

10.5151/2594-357x-12899

Downloads

Abstract

Nove amostras de minerais de ferro foram o objeto deste trabalho que buscou correlacionar sua depressão com amido e carboximetil celulose versus parâmetros mineralógicos e morfológicos das mesmas. Amostras que apresentaram maior conteúdo de hematita compacta (HC) e menor tamanho de cristal apresentaram elevada afinidade pelo coletor, exigindo uma ação depressora mais eficiente com o intuito de minimizar sua tendência natural a flotação e, conseqüentemente, reduzir o teor de Fe no rejeito da flotação. Comportamento distinto foi apresentado por amostras com menor percentual de HC, maior tamanho de cristal e maior conteúdo de hematita martítica, magnetita e goethita. O amido de milho convencional se mostrou capaz de realizar ação depressora sobre todas as amostras, exceto sobre aquelas que se mostraram mais ricas em hematita compacta (HC). Tais hematitas podem ser chamadas de “problemáticas”, visto que interagem fortemente com o coletor e apresentam deficiência de serem deprimidas pelo amido, exigindo elevadas dosagens para minimização de sua tendência natural a flotação. Carboximetil celulose não apresentou ação depressora sobre nenhuma das amostras estudadas. A flotabilildade das amostras ricas em HC ́s pode ser minimizada pela ação do amido de milho condicionado em pH 8,0-8, 5, o que poderá ser traduzido em ganhos de recuperação metálica na flotação.

 

Nine samples of Fe-bearing minerals from several mines of CVRD were the object of this work, which aimed to make a correlation between mineralogy plus morphology versus flotation depression by starch and carboxy methyl cellulose. The samples that exhibited the highest content in compact hematite (HC) and smaller crystal size presented the highest flotation response with cationic collector, demanding stronger action from depressants in order to inhibit their high natural flotation response and, thus, reduce Fe content in the tailings. Different behavior was shown by samples composed of lower content of HC, larger crystal size and higher content of martitic hematite, magnetite and goethite. They did not demand strong action from depressants. Corn starch was able to depress all the samples, except those that exhibit high content of HC. The latter samples could be regarded as “problematic” because they are able to interact strongly with collector and demand high dosage of depressant to accomplish full depression. Carboxy methylcellulose did not show depressive action on any of the studied Fe-beraring minerals. Flotation response of the samples, which are rich in HC, could be minimized by the action of starch conditioned in pH 8.0-8.5, increasing Fe recovery in the process.

Keywords

Hematita; Amido; Flotação; Depressão; Morfologia.

Hematite; Starch; Flotation; Depression; Morphology.

How to refer

Ferreira, Antônio Delfonso; Filho, Laurindo de Salles Leal; Martins, Marisa; Lima, Neymayer Pereira. DEPRESSÃO DE MINERAIS DE FERRO: INFLUÊNCIA DA MINERALOGIA, MORFOLOGIA E pH DE CONDICIONAMENTO , p. 486-494. In: 37º Redução e 8º Minério de Ferro, São Luís - MA, 2007.