Proceedings of ABM Annual Congress


ISSN 2594-5327

77º Congresso Anual da ABM - Internacional vol. 77, num.77 (2024)


Title

DESENVOLVIMENTO DE ROCHA ARTIFICIAL COM RESÍDUO INDUSTRIAL REFORÇADA COM ESCAMA DE PIRARUCU

DEVELOPMENT OF ARTIFICIAL STONE WITH INDUSTRIAL WASTE REINFORCED WITH ARAPAIMA SCALE

DOI

10.5151/2594-5327-41325

Downloads

Abstract

O OBJETIVO DO PRESENTE TRABALHO FOI AVALIAR A INFLUêNCIA DE ESCAMAS JOVENS DE PIRARUCU NO REFORçO DE PEDRAS ARTIFICIAIS CONFECCIONADAS COM Pó DE PEDREIRA E RESINA EPóXI, PELO PROCESSO DE VIBRAçãO, COMPRESSãO E VáCUO. O RESíDUO FOI DIVIDIDO EM TRêS FAIXAS GRANULOMéTRICAS PELO MéTODO DE PENEIRAMENTO: GROSSO E MéDIO (Pó DE PEDREIRA) E FINO (QUARTZITO). OS DADOS FORAM TRATADOS POR MEIO DE ANáLISE ESTATíSTICA. AS PROPORçõES OBTIDAS FORAM 5, 7 E 8 (50% GROSSO E MéDIO), (33% GROSSO, MéDIO E FINO) E (67% GROSSO, 17% MéDIO E 16% FINO). AS 3 COMPOSIçõES DESENVOLVIDAS FORAM SUBMETIDAS AO TESTE DE íNDICE FíSICO. O RESULTADO OBTIDO CLASSIFICOU A COMPOSIçãO 7 PARA A INCORPORAçãO DE ESCAMAS DE PIRARUCU, E FORAM REALIZADOS OS ENSAIOS DE íNDICE FíSICO, FLEXãO E IMPACTO IZOD PARA CARACTERIZAçãO DA PEDRA DESENVOLVIDA. OS RESULTADOS OBTIDOS INDICAM QUE A PEDRA ARTIFICIAL COM ESCAMA DE PIRARUCU APRESENTOU POROSIDADE 0,67% MAIOR QUE AQUELA SEM ESCAMA, INDICANDO FALTA DE ADERêNCIA DA ESCAMA COM OS RESíDUOS. A RESISTêNCIA MECâNICA FOI MAIOR, 34,7 ±2,7 MPA DEVIDO àS ESCAMAS DO PIRARUCU TEREM ALTA RESISTêNCIA. A ENERGIA DE IMPACTO DO I FOI DE 28,3±4,6 J/M PARA A PEDRA ARTIFICIAL ESCAMADA E 24,1 ±4,9 J/M PARA SEM ESCAMA

 

THE OBJECTIVE OF THE PRESENT WORK WAS TO EVALUATE THE INFLUENCE OF YOUNG SCALES OF ARAPAIMA GIGAS ON THE REINFORCEMENT OF ARTIFICIAL STONES MADE WITH QUARRY DUST AND EPOXY RESIN, BY THE PROCESS OF VIBRATION, COMPRESSION AND VACUUM. THE RESIDUE WAS DIVIDED INTO THREE GRANULOMETRIC RANGES BY THE SIEVING METHOD: COARSE AND MEDIUM (QUARRY DUST) AND FINE (QUARTZITE). DATA WERE TREATED THROUGH STATISTICAL ANALYSIS. THE PROPORTIONS OBTAINED WERE 5, 7 AND 8 (50% COARSE AND MEDIUM), (33% COARSE, MEDIUM AND FINE) AND (67% COARSE, 17% MEDIUM AND 16% FINE). THE 3 DEVELOPED COMPOSITIONS WERE SUBMITTED TO THE PHYSICAL INDEX TEST. THE RESULT OBTAINED CLASSIFIED THE COMPOSITION 7 FOR THE INCORPORATION OF ARAPAIMA SCALES, AND THE PHYSICAL INDEX, BENDING AND IZOD IMPACT TESTS WERE PERFORMED TO CHARACTERIZE THE DEVELOPED STONE. THE RESULTS OBTAINED INDICATE THAT THE ARTIFICIAL STONE WITH PIRARUCU SCALE HAD A POROSITY OF 0.67% GREATER THAN THE ONE WITHOUT SCALE, INDICATING LACK OF ADHESION OF THE SCALE WITH THE RESIDUES. THE MECHANICAL STRENGTH WAS HIGHER, 34.7 ±2.7 MPA DUE TO THE ARAPAIMA SCALES HAVING A HIGH STRENGTH. THE IMPACT ENERGY OF IZOD WAS 28.3±4.6 J/M FOR THE SCALED ARTIFICIAL STONE AND 24.1 ±4.9 J/M FOR THE SCALELESS STONE

Keywords

Rocha Artificial; Finos de Brita; Quartzito; Escama de Pirarucu

Artificial stone; fine gravel; quartzite; arapaima scales.

How to refer

COSTA, ELAINE APARECIDA SANTOS CARVALHO; MIRANDA, RAFAEL BITTENCOURT; LIRIO, JOSÉ LUCAS DECOTÉ DE CARVALHO; GOMES, MARIA LUIZA PESSANHA MENEZES; LOPERA, HENRY ALONSO COLORADO; MONTEIRO, SÉRGIO NEVES; VIEIRA, CARLOS MAURÍCIO FONTES. DESENVOLVIMENTO DE ROCHA ARTIFICIAL COM RESÍDUO INDUSTRIAL REFORÇADA COM ESCAMA DE PIRARUCU , p. 2984-2996. In: 77º Congresso Anual da ABM - Internacional, São Paulo, Brasil, 2024.
ISSN: 2594-5327 , DOI 10.5151/2594-5327-41325