Abstract

A caldeira de recuperação de calor de gás de coqueria, denominada caldeira 22, foi submetida à inspeção e reparo conforme os dispostos na NR13 em função de falhas repetitivas que levaram a uma perda repentina de nível de água no tubulão de vapor da Caldeira. O equipamento foi inspecionado levando em consideração técnicas qualitativas e quantitativas de inspeção de equipamento, o que gerou a possibilidade de especificar o reparo. Através do reparo foi possível liberar a caldeira para produção de vapor. Com os dados da inspeção foi realizada uma análise de falha por um grupo multidisciplinar com objetivo de determinar a causa raiz dos modos de falhas detectados durante a inspeção do equipamento: espessura de isolamento térmico inadequado e operação inadequada após detecção de vazamento de água no equipamento. Ações de controle foram definidas e replicadas para as outras caldeiras dessa coqueria. Assim sendo a caldeira 22 está operando em segurança conforme especificação do projeto e com os reparos preventivos já determinados.

 

The heat recovery boiler in the Coke Plant, called 22, was subjected to inspection and repair set forth in NR13 because of repeated failures which led to sudden loos of water level in the boiler drum. The boiler was inspected taking into account qualitative and quantitative equipment inspection techniques, which generated the possibility of specifying the repair. Through the repair it was possible to release the boiler for steam production. With the inspection information, a failure analysis was performed by a multidisciplinary group to determine the root cause of failure modes detected during equipment inspection: inadequate thermal insulation thickness and inadequate operation after detection of water leakage in the equipment. Control actions were defined and replicated to the other boilers in this coke plant. Then boiler 22 is operating safely according to the project specification and with the preventive repairs already determined.

Keywords

caldeira de recuperação de calor, inspeção e reparo de caldeira, NR13, analise de falha

Heat recovery boiler, Boiler inspection and repair, NR13, Failure analysis

How to cite

Ferreira, Davi Fernando Soares; Souza, Kallin de; Materna, Fernando Gonçalves; José Gonçalves Pacheco Júnior; Magalhães, Igor Striotto Kramer. INSPEÇÃO, REPARO E ANALISE DE FALHA EM UMA CALDEIRA DE RECUPERAÇÃO DE CALOR DE GÁS DE COQUERIA, p. 2178-2189. In: 72nd ABM Annual Congress, São Paulo, 2017.
ISSN: 2594-5327, DOI 10.5151/1516-392X-30632