Abstract

Nas linhas de zincagem nº1 e nº2 da Companhia Siderúrgica Nacional (CSN) não existe seção de limpeza, sendo necessário efetuar a limpeza no forno de recozimento, na seção do pré-aquecimento com temperatura acima de 620°C, onde ocorre a volatização dos fluidos de laminação e impurezas existentes na chapa. Durante o processo de limpeza, ocorre o surgimento do pick-up nos rolos do forno. O pick-up é a ancoragem da carepa superficial (impurezas) da chapa na superfície do rolo. O pick-up ao aderir no corpo do rolo provoca desvios e ocorrências de qualidade na chapa durante o processo de recozimento. Este trabalho busca eliminar o pick-up nos rolos do forno para reduzir os desvios e ocorrências de qualidade provocado por ele. Serão abordados os motivos da formação do pick-up, bem como os custos operacionais e de manutenção. O trabalho mostrará as ações implantadas como solução e os resultados obtidos. Ao final do trabalho será apresentado.

 

In galvanizing lines No. 1 and No. 2 of the National Steel Company (CSN) no cleaning section, being necessary to make cleaning the oven annealing, the section of the pre-heating temperature above 620°C, where volatilization occurs fluid lamination and impurities on the plate. During the cleaning process, there is the appearance of the pick-up rollers of the furnace. Pick-up is the anchoring of surface russeting (dross) of the plate on the roller surface. The pick-up to join the body of the roller causes deviations and occurrences of quality on the plate during the annealing process. This work seeks to eliminate the pick-up coils in the furnace to reduce the instances of deviations and quality caused by it. It will examine the reasons for the formation of the pick-up and operational costs and maintenance. The work shows the actions implemented as a solution and results. At the end of the work will be presented to verify the effectiveness and standardization of the deployed solution.

Keywords

Rolos de forno horizontal; Pick-up; Carepa superficial.

Horizontal furnace rolls; Pick-up; Superficial corrosion.

How to refer

Esquerdo, Emilio Augusto Ferreira; Lima, Reginaldo Cardoso de; Carneiro, Valdeci Oliveira; Lima, Wendel Silva. REDUÇÃO DOS DESVIOS DE QUALIDADE CAUSADOS PELOS ROLOS DO FORNO DE RECOZIMENTO NA LZC 1 E 2 DA COMPANHIA SIDERURGICA NACIONAL , p. 2447-2458. In: 67º Congresso da ABM - Internacional / 12º ENEMET - Encontro Nacional de Estudantes de Engenharia Metalúrgica, de Materiais e de Minas, Rio de Jabeiro, 2012.