Title

USO DO IMAGEJ NA METALOGRAFIA QUANTITATIVA

THE USE OF IMAGEJ IN QUANTITATIVE METALLOGRAPHY

Authorship

DOI

10.5151/2594-4711-41278

Downloads

4 Downloads

Abstract

A METALOGRAFIA QUANTITATIVA DESEMPENHA UM PAPEL CRUCIAL NA CIêNCIA DOS MATERIAIS E NA INDúSTRIA, FORNECENDO INFORMAçõES DETALHADAS DA MICROESTRUTURA QUE, CONSEQUENTEMENTE, ESTãO RELACIONADAS COM AS PROPRIEDADES DOS MATERIAIS. ESSE ARTIGO TEVE COMO FINALIDADE DESCREVER UM MéTODO PRáTICO DO USO DO PROGRAMA DE PROCESSAMENTO DE IMAGEM DE CóDIGO ABERTO, IMAGEJ, NO CAMPO DA METALOGRAFIA QUANTITATIVA, A FIM DE EXPANDIR E OTIMIZAR OS ESTUDOS NESSA áREA COM OS VASTOS RECURSOS DESSA VERSáTIL FERRAMENTA GRATUITA. DESSE MODO, COM A METODOLOGIA DESENVOLVIDA, TORNOU-SE POSSíVEL FAZER O CáLCULO DO TAMANHO DE GRãOS, DA áREA DOS POROS E DA FRAçãO VOLUMéTRICA DAS FASES DE UMA MICROESTRUTURA DE FORMA SIMPLES E RáPIDA, COM O USO DE MéTODOS PRáTICOS E AUTOMATIZADOS, SUPORTADOS PELA UTILIZAçãO DE PLUGINS, COMO O JPOR, E PELA CONFECçãO DE TUTORIAIS DETALHADOS E DIDáTICOS.

 

QUANTITATIVE METALLOGRAPHY REPRESENTS A CRUCIAL ROLE IN MATERIALS SCIENCE AND INDUSTRY BY PROVIDING DETAILED INFORMATION ABOUT MICROSTRUCTURES, WHICH ARE CONSEQUENTLY RELATED TO THE PROPERTIES OF MATERIALS. THIS ARTICLE’S GOAL IS TO DESCRIBE A PRACTICAL METHOD FOR USING THE OPEN-SOURCE IMAGE PROCESSING PROGRAM, IMAGEJ, IN THE FIELD OF QUANTITATIVE METALLOGRAPHY, IN ORDER TO EXPAND AND OPTIMIZE STUDIES IN THIS AREA WITH THE VAST RESOURCES OF THIS VERSATILE AND FREE TOOL. THUS, WITH THE DEVELOPED METHODOLOGY, IT HAS BECOME POSSIBLE TO CALCULATE GRAIN SIZE, PORE AREA, AND THE VOLUMETRIC FRACTION OF PHASES IN A MICROSTRUCTURE IN A SIMPLE AND QUICK WAY, USING PRACTICAL AND AUTOMATED METHODS SUPPORTED BY THE USE OF PLUGINS SUCH AS JPOR AND THE CREATION OF DETAILED AND DIDACTIC TUTORIALS.

Keywords

ImageJ; Metalografia quantitativa; Microestrutura.

ImageJ; Quantitative metallography; Microstructure.

How to cite

RIOS, LUIZ FERNANDES; SANTANA, ALISSON NUNES; LIMA, GABRIEL AIRES; BARBOSA, DANIEL MACHADO; ROCHA, LUCAS FREITAS DA; BARBOSA, ARTUR TIMBÓ; GARCIA, JULIANNA MAGALHAES; BRANDÃO, LUIZ PAULO MENDONÇA; Dionathan Trindade Boor; SOUSA, TALITA GAMA DE. USO DO IMAGEJ NA METALOGRAFIA QUANTITATIVA, p. 490-495. In: 22nd Enemet - National Meeting of Metallurgical, Materials and Mining Engineering Students, São Paulo, Brasil, 2024.