Abstract

Devido à interação das linhas flexíveis (LF) com solo marinho, há uma forte redução da espessura dessas linhas na parte inferior. Para amenizar esse problema são usadas proteções em forma de calhas bipartidas que são fixadas nas regiões de desgaste intenso através de cintas metálicas. O presente trabalho tem como objetivo identificar os principais mecanismos de degradação de proteções linhas flexíveis de extração de petróleo na região de toque com o leito marinho – TDP (Touch Down Point). Os mecanismos de desgaste foram analisados em amostras removidas após 44 meses de operação de uma LF, correspondente à região de TDP, (poço Marlin 37, plataforma P- 19, linha de injeção de água, diâmetro de 6 polegadas). Imagens de perfis e microscopias eletrônicas de varredura de superfícies desgastadas foram observados e encontrou-se, que a degradação desses componentes se dá, basicamente, pela ocorrência de grandes eventos de riscamento por deslizamento de partículas duras. Outros mecanismos são observados, mas com efeitos minoritários sobre a taxa de desgaste do componente.

 

On inspection of flexible risers, scratches and a significant reduction of the riser protection layer were observed. These damages were found to be related to the relative movement of the pipe in the area of the touchdown point (TDP). In order to reduce this problem the risers have being coated externally with plaques of polyurethane. The objective of this work is to investigate the main mechanisms of degradation of the flexible lines’s protections. The consuming mechanisms had been analyzed in samples removed after 44 months of operation of a LF, correspondent to the TDP region, (well Marlin 37, P-19 platform, line of water injection, diameter 6 inch). Images of sections and worn surfaces were observed on a scanning electron microscope for analysis of the degradation of the gutters. Using SEM imaging, it was found, that three wear eventes exist. However, the most significant wear mechanisms is the scratching for elements with less acute tips.

Keywords

Degradação; Linhas flexíveis; TDP.

Degradation; Flexible lines; TDP.

How to refer

Paes, Marcelo Torres Piza; Motta, Antônio Marcos Rego; Marinho, Ricardo Reppold; Morais, Juliano Oséias de; Franco, Sinésio Domingues. MECANISMOS DE DEGRADAÇÃO DE PROTEÇÕES DE LINHAS FLEXÍVEIS NA REGIÃO DO TDP , p. 3859-3868. In: 61º Congresso Anual da ABM, Rio de Janeiro, 2006.
ISSN: 2594-5327 , DOI 10.5151/2594-5327-0432